Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.96 GPa | 1880 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 12.96 GPa | 1880 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Modulus | 12.96 GPa | 1880 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON AE004 ABS (Asia Pacific) LNP* STAT-KON* AE004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 12.96 GPa | 1880 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WF006L PBT LNP* THERMOCOMP* WF006L is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this material is: Low Extractible. |