Mechanical Properties Metric English Comments
Tensile Modulus 19.4 GPa
2810 ksi
ASTM D638
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Tensile Modulus 19.4 GPa
2810 ksi
ASTM D638
Unitika RUN35-TA Light resistant PA6, Dry
Light resistant and internalInformation provided by Unitika Ltd.