Polymer Property : Tensile Modulus = 1941 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.38 GPa
1941 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.