Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and..
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun..
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid..
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M..
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ UL 00728FF Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid..
Tensile Modulus 0.0159 GPa
2.30 ksi
(0.2 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 02528CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 02528CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: YesFree ..
Tensile Modulus 0.0159 GPa
2.30 ksi
Molded Properties; ISO 527-2/1
ExxonMobil Escorene™ FL 00328 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00328 is a copolymer of ethylene and vinyl acetate offering low gel. Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation. Machine..