Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.10 - 2.45 GPa | 305 - 355 ksi | |
Addcomp PRIEX® Ionomer 42101 PP homopolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Tensile Modulus | 2.10 - 2.45 GPa | 305 - 355 ksi | |
Addcomp PRIEX® Ionomer 40101 PP homopolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |