Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2.63 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.63 GPa
381 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific)
Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance..
Tensile Modulus 2.63 GPa

@Temperature 23.0 °C
381 ksi

@Temperature 73.4 °F
ASTM D638
PolyOne Geon™ CPVC EC050 Polyvinyl Chloride, Chlorinated (CPVC)
The Geon EC050 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon EC050 demonstrates ease of processing and excellent t..
Tensile Modulus 2.63 GPa

@Temperature 23.0 °C
381 ksi

@Temperature 73.4 °F
ASTM D638
PolyOne Geon™ CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC)
The Geon EC950 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC950 demonstra..
Tensile Modulus 2.63 GPa
381 ksi
Molded; ASTM D882
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Tensile Modulus 2.63 GPa
381 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility
Tensile Modulus 2.63 GPa
381 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX12411C PC