Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2.84 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.84 GPa
412 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
Tensile Modulus 2.84 GPa
412 ksi
ASTM D638
Nilit Polynil® P200 High Viscosity Nylon 66
Description: High viscosityApplication: Semi-finished and FilmInformation provided by NILIT.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX00887C PC
LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly
LNP* THERMOCOMP* KZ001L is a compound based on Acetal Copolymer resin containing 5% Milled Glass. Added features of this material include: Low Extractible.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL LTA1350 PPE+PS
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Tensile Modulus 2.84 GPa
412 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 2.84 GPa
412 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East)
Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Tensile Modulus 2.84 - 3.117 GPa
412 - 452.1 ksi
ASTM D638
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System
Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/..
Tensile Modulus 2.84 GPa

@Temperature -40.0 °C
412 ksi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Tensile Modulus 2.84 - 3.048 GPa
412 - 442.1 ksi
90 Minute UV Cure; ASTM D638
3D Systems Accura® SI 40 Plastic for the SLA® 500 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
Tensile Modulus 2.84 GPa
412 ksi
Abatron AboCast 8103-22 High-Performance Dielectric Epoxy
AboCast 8103-22 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system is used in..
Copyright © lookpolymers.com All Rights Reserved