Polymer Property : Tensile Modulus = 20.35 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 20.35 GPa
2952 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA
LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.