Polymer Property : Tensile Modulus = 2028 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 13.98 GPa
2028 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Tensile Modulus 13.98 GPa
2028 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6