Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 2050 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 14.1 GPa
2050 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific)
DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength
Tensile Modulus 14.1 GPa
2050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear
LNP* THERMOCOMP* OF008 is a compound based on PPS - Linear resin containing 40% Glass Fiber.
Tensile Modulus 14.1 GPa
2050 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear
LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare.
Tensile Modulus 14.1 GPa
2050 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
Tensile Modulus 14.1 GPa
2050 ksi
ISO 527-2
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..