Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.19 GPa | 2058 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |