Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific)
LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by ..
Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00BS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00BS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific)
LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Modulus 21.37 GPa
3099 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.