Polymer Property : Tensile Modulus = 21.77 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 21.77 GPa
3157 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific)
LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..