Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.8 GPa | 2150 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON 9X08403C Liquid Crystal Polymer (LCP) LNP* STAT-KON* 9X08403C is a compound based on Liquid Crystal Polymer (LCP) resin containing Carbon Fiber. Added features of this material are: Clean Compounding System, High Temperature, Flame Re.. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass.. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Black Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Black is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, .. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H NT Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H NT is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. .. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Tensile Modulus | 14.8 GPa | 2150 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 50 NOIR T6LD Nylon 12, 50% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-090,GF50Rigid grade with glass fiber (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |