Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.86 GPa | 2155 ksi | ASTM D638 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Tensile Modulus | 14.86 GPa | 2155 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE004ER PC LNP* STAT-KON* DE004ER is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added featuresof this material include: Electrically Conductive, Easy Molding, Mold Release. |