Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 216 GPa | 31300 ksi | |
Toho Tenax Besfight® MC Type II (12,000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Tensile Modulus | 216 GPa | 31300 ksi | |
Toho Tenax Besfight® MC Type II (3000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |
|||
Tensile Modulus | 216 GPa | 31300 ksi | |
Toho Tenax Besfight® MC Type II (6000 Filament) Nickel Coated Carbon Fiber Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec.. |