Mechanical Properties Metric English Comments
Tensile Modulus 15.14 GPa
2196 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp EF008E PEI
LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas..