Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.155 GPa
22.5 ksi
ASTM D638
Spartech SP-1310 Polyolefin Sheet
Description: Polyolefin SheetInformation provided by Spartech.
Tensile Modulus 0.155 GPa

@Temperature 120 °C
22.5 ksi

@Temperature 248 °F
ISO Data
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications.