Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 23.5 GPa | 3410 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60 Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory.. |
|||
Tensile Modulus | 23.5 GPa | 3410 ksi | transverse; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Tensile Modulus | 23.5 GPa | 3410 ksi | transverse; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |
|||
Tensile Modulus | 23.5 GPa | 3410 ksi | ISO 527-1 |
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced PEEK-CF30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 23.5 GPa | 3410 ksi | transverse; ISO 527-4/5 |
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea.. |