Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.165 GPa | 23.9 ksi | TD; ASTM D882-A |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Tensile Modulus | 0.165 GPa | 23.9 ksi | TD; ASTM D882-A |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |
|||
Tensile Modulus | 0.165 GPa | 23.9 ksi | ISO 527-1/-2 |
DSM Arnitel® PL461 Injection Molding Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.165 GPa | 23.9 ksi | ISO 527-1/-2 |
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.165 GPa @Temperature 23.0 °C |
23.9 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Tensile Modulus | 0.165 GPa | 23.9 ksi | 1 mm/min |
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Tensile Modulus | 0.165 GPa | 23.9 ksi | ASTM D882 |
DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A one-side PVDC-coated LLDPE sealant film, which provides excellent barrier properties, while retaining the outstanding physical and seal strength characte.. |