Mechanical Properties Metric English Comments
Tensile Modulus 16.2 GPa
2350 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Tensile Modulus 16.2 GPa
2350 ksi
ISO 527 Type 1A
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Modulus 16.2 GPa
2350 ksi
ASTM D638
Plenco 6990 Phenolic, Briquette, Injection Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Tensile Modulus 16.2 GPa
2350 ksi
1mm/min; ISO 527
BASF Petra® 140 45% Glass Filled PET
Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex..