Tensile Modulus 16.21 GPa
2351 ksi
ASTM D-638
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.