Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.165 GPa | 24.0 ksi | Secant; ASTM D638 |
M. Holland Company LD300 LDPE
(discontinued **) Features: High ESCR (Stress Crack Resist.), Good Processability, Low Temp. StrengthUses: Closures, Electrical Parts, Household GoodsApprovals: FDA 21 CFR 177.1520(c) 2.2Processing Method: Injection .. |
|||
Tensile Modulus | 0.165 GPa | 24.0 ksi | ASTM D638 |
3M Dyneon™ CCM605 PTFE, 25% Glass Filled
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Tensile Modulus | 0.165 GPa | 24.0 ksi | ASTM D1709 |
Westlake EC483 Low Density Polyethylene WESTLAKE low-density polyethylene EC483 is recommended for use in the boardstock coating industry. This resin has low neck-in, good heat sealing properties, and good drawdown characteristics.Applica.. |