Polymer Property : Tensile Modulus = 24.61 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 24.61 GPa
3569 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66
LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r..
Tensile Modulus 24.61 GPa
3569 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66
LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive.