Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.5 GPa @Temperature 21.1 °C |
2400 ksi @Temperature 70.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, Silica Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
0° Direction, Dry; 325°F Autoclave; ASTM D638 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
0° Direction, Dry; 8HS form; ASTM D638 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, NARC/CYDSA Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.9 °C |
2400 ksi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 120 E-Glass Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Tensile Modulus | 16.5 GPa | 2400 ksi | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |