Mechanical Properties Metric English Comments
Tensile Modulus 16.75 GPa
2429 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON Valox_VCF2020 PET
LNP* Stat-kon* Valox_VCF2020 compound is a 20% carbon fiber reinforced PET. Conductive applications.