Tensile Modulus 245 GPa
35500 ksi
Typical fiber property; Chord 6000-1000
Hexcel® HexTow™ AS4D Carbon Fiber
HexTow™ AS4D carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 12,000 (12K) filament count tows. The fiber has been surface treated and can be sized to improve ..