Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 18.1 GPa | 2630 ksi | 1mm/min; ISO 527 |
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |