Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 265 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 1.83 GPa
265 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal
LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Tensile Modulus 1.83 GPa
265 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Tensile Modulus 1.83 GPa
265 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
10 mm/min; SABIC - Japan Method
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
10 mm/min; SABIC - Japan Method
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
10 mm/min; SABIC - Japan Method
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Tensile Modulus 1.83 GPa
265 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Tensile Modulus 1.83 GPa
265 ksi
ASTM Test
Styrolution Luran® S 797 SE ASA
Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided ..
Tensile Modulus 1.83 GPa
265 ksi
ASTM Data
Styron Magnumâ„¢ 275 ABS, Low Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Modulus 1.83 GPa
265 ksi
ASTM Data
Styron Magnumâ„¢ 8325 ABS, Sheet Coextrusion Grade
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Tensile Modulus 1.83 GPa
265 ksi
ASTM D638
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene
Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances..
Copyright © lookpolymers.com All Rights Reserved