Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.84 GPa | 267 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY CR3020 ASA Low-gloss ASA for profile and capstock applications |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Konduit MT00EL PP LNP* Konduit* MT00EL is a Polypropylene base resin with thermal fillers. Characteristics of this grade are Thermal Conductivity and it is Low Extraactible.This data was supplied by SABIC-IP for th.. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | ISO 527 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY NX13401 PC+ABS LNP* STAT-LOY* NX13401 is a compound based on PC+ABS blend. Added features of this material include: Antistat, Flame Retardant, Excellent Release. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | Secant; ISO 527-2 |
ExxonMobil Exxtral™ BMU 234 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive exterior parts and high stiffness, high impact and good dimensional stability.Availability: Africa & Middle Ea.. |
|||
Tensile Modulus | 1.84 GPa @Temperature 110 °C |
267 ksi @Temperature 230 °F |
50%RH; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | same value from ASTM and ISO test. |
BASF Capron® BU50I Ultratough Nylon 6 (Dry)
(discontinued **) Capron Ultratough Nylon BU50I is an unfilled nylon 6 product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme low temperature tolerance of Ultratough Nylon BU5.. |
|||
Tensile Modulus | 1.84 GPa | 267 ksi | 1mm/min |
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Modulus | 1.84 GPa @Temperature 30.0 °C |
267 ksi @Temperature 86.0 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |