Polymer Property : Tensile Modulus = 27.16 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 27.16 GPa
3939 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON OE004AE PPS - Branched
LNP STAT-KON* OE004AE is a compound based on PPS - Branched resin containing 20% Carbon Fiber. Added features of this material are: Easy Molding, Electrically Conductive.