Polymer Property : Tensile Modulus = 2764 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 19.06 GPa
2764 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA
LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable.