Tensile Modulus 1.945 GPa
282.1 ksi
Z; ASTM D638
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..