Mechanical Properties Metric English Comments
Tensile Modulus 19.7 GPa
2860 ksi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope..
Tensile Modulus 19.7 GPa

@Temperature 23.0 °C
2860 ksi

@Temperature 73.4 °F
4; ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention..
Tensile Modulus 19.7 GPa
2860 ksi
5 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber
KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic..
Tensile Modulus 19.7 GPa

@Temperature 23.0 °C
2860 ksi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..