Tensile Modulus 2.013 - 2.187 GPa
292.0 - 317.2 ksi
ASTM D638M
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer
Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app..