Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 20.3 GPa | 2940 ksi | ISO 527-1,2 |
Qualchem Danamid FCF-20 Polyamide 6, 20% Carbon Fiber Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 20.3 GPa | 2940 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Tensile Modulus | 20.3 GPa | 2940 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Europe-Africa-Middle East) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Tensile Modulus | 20.3 GPa | 2940 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Tensile Modulus | 20.27 GPa | 2940 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Modulus | 20.27 GPa | 2940 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |