Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.137 GPa | 455.0 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22XXC Acetal Copolymer LNP* LUBRICOMP* KAL22XXC is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 3.137 GPa | 455.0 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Tensile Modulus | 3.137 GPa | 455.0 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific) LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |