Polymer Property : Tensile Modulus = 3.47 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.47 GPa
503 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Tensile Modulus 3.47 GPa
503 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS
LNP THERMOCOMP* NF001 is a compound based on PC+ABS resin containing 5% Glass Fiber.
Tensile Modulus 3.47 GPa
503 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS
LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber.