Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.56 GPa | 517 ksi | TD; ASTM D638 |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Tensile Modulus | 3.56 GPa | 517 ksi | Y direction; 0.1/min strain rate; ASTM D638 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Tensile Modulus | 3.56 GPa | 516 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8408 PPE+PA Noryl GTX* GTX8408 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is glass filled and suitable for injection molding. The elongation of this material is higher than GTX8410W.. |
|||
Tensile Modulus | 3.56 GPa | 517 ksi | Storage |
Epoxy Technology EPO-TEK® 353ND Black High Temperature Epoxy Product Description: EPO TEK® 353ND Black is a a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applicationsAdvantages & Application Notes: EPO T.. |
|||
Tensile Modulus | 3.56 GPa | 517 ksi | Storage |
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra.. |