Polymer Property : Tensile Modulus = 3.9490 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 3.9490 GPa
572.75 ksi
Storage
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..