Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.225 GPa | 32.6 ksi | ISO 527-1/-2 |
DSM Arnitel® EB500 50 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.225 GPa | 32.6 ksi | ISO 527-1/-2 |
DSM Arnitel® EB500 Polyether Ester Elastomer (European and Asian Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.225 GPa | 32.6 ksi | ISO 527 |
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey Information provided by Eurotec® |