Polymer Property : Tensile Modulus = 32.8 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 32.8 GPa
4760 ksi
ASTM D638
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..