Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.233 GPa | 33.8 ksi | TD |
Kuraray HYBRAR® CF1 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Tensile Modulus | 0.233 GPa @Temperature 160 °C |
33.8 ksi @Temperature 320 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |