Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-400 1K HTA-7W EP01 Continuous Filament Carbon Fiber Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 12K HTA-7C NS01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 3K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 3K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 3K HTA-7W EP01 Continuous Filament Carbon Fiber Standard Modulus; Twisted; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Tensile Modulus | 234 GPa | 34000 ksi | |
Toho Tenax Besfight® G30-500 6K HTA-7C EP03 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |