Mechanical Properties Metric English Comments
Tensile Modulus 23.54 GPa
3414 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP STAT-KON OE006C1 PPS - Linear
LNP* STAT-KON* OE006C1 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.