Polymer Property : Tensile Modulus = 34800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 240 GPa
34800 ksi
Toho Tenax Besfight® STS 24K HTA-7C F301 Continuous Filament Carbon Fiber
Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car..