Polymer Property : Tensile Modulus = 3610 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 24.9 GPa
3610 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036L is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Modulus 24.9 GPa
3610 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East)
LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive .
Tensile Modulus 24.9 GPa
3610 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6
LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive.