Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 24.95 GPa | 3619 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Modulus | 24.95 GPa | 3619 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |