Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Amber 9360 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Amber 9375 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging 2710 Polyvinyl Chloride, Rigid (PVC, Rigid) This product is available in opaque and transparent colors.Information provided by PolyOne |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | ASTM D638 |
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7100 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded au.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus. |
|||
Tensile Modulus | 2.53 GPa @Temperature -100 °C |
367 ksi @Temperature -148 °F |
Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min |
Arkema Group Nakan® RPX 301 L PVC, Rigid Extrusion Grade NAKAN RPX 301 L is a rigid polyvinyl chloride compound developed for extrusion of transparent profiles for outdoor applications.ISO data provided by the manufacturer, Arkema. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | same value from ASTM and ISO test. |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Tensile Modulus | 2.53 GPa | 367 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FP5140HF PPE+PS Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u.. |