Mechanical Properties Metric English Comments
Tensile Modulus 37.9 GPa
5500 ksi
5.1 mm/min; ASTM D638
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Information provided by PolyOne
Tensile Modulus 37.9 GPa
5500 ksi
5.1 mm/min; ASTM D638
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..